Kimyoviy tarkibi
Qotishma | element | C | Si | Mn | S | Ni | Fe | Cu |
Monel 400 | Min | 63,0 | 28.0 | |||||
Maks | 0.3 | 0,5 | 2.0 | 0,024 | 2.5 | 34.0 |
Mexanik xususiyatlar
Aolly holati | Mustahkamlik chegarasi Rm Mpa Min | Hosildorlik kuchi RP 0, 2 Mpa Min | Cho'zilish A 5% Min |
Yechim | 745 | 325 | 40 |
Jismoniy xususiyatlar
Aolly holati | Kuchlanish kuchi Rm Mpa Min. | Chiqish kuchi RP 0. 2 Mpa Min. | Cho'zilish A 5 % |
tavlangan | 480 | 170 | 35 |
Standart
Rod, bar, sim va zarb zahiralari- ASTM B 164 (tayoq, novda va sim), ASTM B 564 (zarb)
Plita, varaq va tasma-, ASTM B 127, ASME SB 127
Quvur va quvur- ASTM B 165 (choksiz quvur va quvur), ASTM B 725 (payvandlangan quvur), ASTM B 730 (payvandlangan quvur), ASTM B 751 (payvandlangan quvur), ASTM B 775 (payvandlangan quvur), ASTM B 829 (choksiz quvur va Tube)
Payvandlash mahsulotlari- To'ldiruvchi metall 60-AWS A5.14/ERNiCu-7; Payvandlash elektrodi 190-AWS A5.11/ENiCu-7.
Monel 400 ning xususiyatlari
● Yuqori haroratlarda dengiz suvi va bug'ga chidamli
● Tez oqadigan sho'r suv yoki dengiz suviga mukammal qarshilik
● Ko'pgina chuchuk suvlarda stressli korroziya yorilishiga mukammal qarshilik
● Xlorid va gidroflorik kislotalarga ayniqsa chidamli, ular gazsizlanganda
● O'rtacha harorat va konsentratsiyalarda xlorid va sulfat kislotalarga biroz qarshilik ko'rsatadi, lekin bu kislotalar uchun kamdan-kam hollarda tanlangan materialdir.
● Neytral va gidroksidi tuzga mukammal qarshilik
● Xloriddan kelib chiqqan stressli korroziya yorilishiga qarshilik
● Noldan past haroratlardan 1020 ° F gacha bo'lgan yaxshi mexanik xususiyatlar
● Ishqorlarga nisbatan yuqori qarshilik